We manufacture ladles and T-Pot ladles. At present we produce several Vibrocast models, see table, and we continually develop new models based on market requirements. Please contact us for more information.
| MODE | OUTSIDE DIAMETER (MM) | INSIDE DIAMETER (MM) | OVERALL LENGTH (MM) | INSIDE LENGTH (MM | CAPACITY OF STEEL (80%) KG | OUTSIDE DIAMETER (INCH) | INSIDE DIAMETER (INCH) | OVERALL LENGTH (INCH) | INSIDE LENGTH (INCH) | CAPACITY OF STEEL (80%) LBS |
| 6134 | 205 | 170 | 210 | 190 | 20 | 8,1 | 6,7 | 8,3 | 7,5 | 44 |
| 6334 | 230 | 195 | 255 | 235 | 35 | 9,1 | 7,7 | 10,0 | 9,3 | 75 |
| 6009 | 318 | 287 | 308 | 295 | 65 | 12,5 | 11,3 | 12,1 | 11,6 | 145 |
| 5750 | 251 | 225 | 381 | 365 | 65 | 9,9 | 8,9 | 15,0 | 14,4 | 140 |
| 6204 | 340 | 309 | 320 | 307 | 90 | 13,4 | 12,2 | 12,6 | 12,1 | 195 |
| 6032 | 349 | 299 | 440 | 400 | 150 | 13,7 | 11,8 | 17,3 | 15,7 | 330 |
| 6069 | 370 | 320 | 470 | 430 | 175 | 14,6 | 12,6 | 18,5 | 16,9 | 385 |
| 6038 | 415 | 350 | 380 | 345 | 200 | 16,3 | 13,8 | 15,0 | 13,6 | 440 |
| 6045 | 456 | 396 | 595 | 550 | 300 | 18,0 | 15,6 | 23,4 | 21,7 | 660 |
| 6073 | 515 | 435 | 500 | 460 | 300 | 20,3 | 17,1 | 19,7 | 18,1 | 660 |
| 6175 | 574 | 484 | 750 | 690 | 600 | 22,6 | 19,1 | 29,5 | 27,2 | 1320 |