Temperature Measurement

Our thermocouples may be used with our Digiterm 97 temperature measuring instrument and lance.

Digiterm 97 has the following features:

  • Robust Digital LED display (easy to read in foundry conditions)
  • Rechargable battery operated
  • Portable
  • Indicates when the thermocouple is open circuit(broken)
  • Indicates when the temperature plateau is reached
  • Quick response time, typically temperature reading within 4 seconds
  • Suitable for Type R or S thermocouples
  • Temperature range 500-1750ºC
  • Ten reading memory

Brochure Request

Thank you

Your brochure is ready for download.

Download brochure