Slip Plane Material (Mica)

The slip plane is positioned against the coil screed to provide a smooth surface. This is essential for uninhibited reversible movement of the refractory lining caused by its thermal expansion and contraction. The mica also offers a degree of protection against metal penetration.

Mica Mesh
A sandwich of metal mesh between two layers of mica is available which is used in systems that give early warning of metal penetration through a lining.

PRODUCT NAME LENGTH / M WIDTH / M THICKNESS / MM FORM
Mica Sheet 1.2 /1.8 / 2.2 1.0 0.4 sheet
Mica Roll 12.5 1.0 0.3 roll
Mica Glass 20.0 1.0 0.4 roll
Combi-Roll 12.5 1.0 2.0 roll
Mica Foil 20.0 1.0 0.4 roll
Mica Weave 20.0 1.0 0.28 roll