Capital manufactures an extensive range of spinel-forming linings. These have been specifically developed for a variety of metals and some allow for a mixed melting programme. The furnace lining products are complemented by a complete range of toppings, spout, repair, and patching materials.
Capital supply a selection of high performance dry rammed products for vacuum induction melting furnaces to meet the mixture of the master alloy.
• Coral V40 • Coral V40-DT • CoralV43 • Coral V43-DT
Chemically bonded high strength materials compatible with Capital’s dry linings.
High grade fine hydraulic cements.
The slip plane is positioned against the coil screed to provide a smooth surface. This is essential for uninhibited reversible movement of the refractory lining caused by its thermal expansion and contraction. The mica also offers a degree of protection against metal penetration.
A sandwich of metal mesh between two layers of mica is available which is used in systems that give early warning of metal penetration through a lining.
Capital supply a selection of high performance dry rammed products for vacuum induction melting furnaces to meet the mixture of the master alloy.
| Quality | Al₂O₃ | MgO | SiO₂ | CaO | Fe₂O₃ | Description |
| Coral V40 | 38.0 | 58.0 | 2.2 | 1.0 | 0.1 | High performance dry vibratable. |
| Coral V43 | 33.7 | 63.2 | 0.7 | 1.1 | 0.4 | Superior performance providing high resistance to aggressive alloys. |
| Coral V45 | 40.5 | 58.0 | 0.3 | 0.8 | 0.4 | - |
| Product Name | Product Description | Maximum Grain Size / mm | Bond | Maximum Service Temperature / °C |
| Coral V40DT | Dry vibration heat set topping compatible with Coral V40 | 8 | Ceramic | 1700 |
| Coral V43DT | Dry vibration heat set topping compatible with Coral V43 | 8 | Ceramic | 1700 |
| Capram 90 | A family of chemically bonded, high alumina, plastic/plaster refractories. | 5 | Chemical | 1800 |
| Product Name | Product Description | Maximum Grain Size / mm | Bond | Maximum Service Temperature / °C |
| Silkote 90 | High alumina induction furnace coil screed with good applicability and surface finish. | 1 | Hydraulic | 1700 |
| Capscreed | High strength high alumina induction furnace coil screed widely used with push-out furnaces. | 1 | Hydraulic | 1680 |
| Capscreed 96C | High fluidity vibratable coil screed. | 1 / 3 | Hydraulic | 1800 |
| Capgrout G | High alumina, induction furnace coil screed with good usability. | 1 | Hydraulic | 1700 |
| Product Name | Length / m | Width / m | Thickness / mm | Form |
| Mica Sheet | 1.2 /1.8 / 2.2 | 1.0 | 0.4 | sheet |
| Mica Roll | 12.5 | 1.0 | 0.3 | roll |
| Mica Glass | 20.0 | 1.0 | 0.4 | roll |
| Combi-Roll | 12.5 | 1.0 | 2.0 | roll |
| Mica Foil | 20.0 | 1.0 | 0.4 | roll |
| Mica Weave | 20.0 | 1.0 | 0.28 | roll |
| Product Name | Product Description | Bond | Maximum Service Temperature / °C |
| Capram 90FZP | High alumina plastic/plaster refractory. | Chemical | 1700 |
| Capram 90 | Chemically bonded, high alumina, plastic/plaster refractory | Chemical | 1800 |